Name: DIY shrink wrap kit Specification: Handcrafted craft Product features: Enhances hands-on skills and DIY creativityAbility, easy to get started Note: When using the hot air gun, the temperature can be very high., Should be used correctly, do not block the air outlet during use. After using it, let it cool down.Place in a well-ventilated and cool area |


1. Prepare the heat-shrinkable film for gluing
2. Place the heat-shrinkable sheet for glue application on a horizontal surface; if not horizontal, the glue may flow away or be uneven!
3. Use a 5 ml syringe to take an appropriate amount of A glue. In my opinion, heating A glue with hot water makes the bubbles formed when dripping more effective.
Easy to burn)Use a 2.5 ml syringe to extract an appropriate amount of B glue (for example, if A glue is taken 5 ml, then B glue should be taken 2 ml).
PS: B glue is a coagulant. If you find that it sets slowly, please use a little more B glue next time.
4. Mixing: Glass rods, bamboo sticks, etc. can be used for mixing (it must be thoroughly mixed evenly). I mix quickly each time.
In three minutes).
5. Many bubbles may form in the glue after stirring, but that’s fine; they will dissipate on their own after being left to stand for a while.
To the transparent state.
Because the freshly prepared glue is quite thin, wait for 10–20 minutes until it becomes slightly thicker before dripping (specifically)
The time depends on the temperature at that moment), and the crystal surface resulting from this will be different
It looks good when full. The prepared glue should be used up within half an hour, as if left too long, the glue starts
It becomes solid and can't drip anymore.
6. Within 24 hours after滴ing, bubbles may continue to form continuously; be aware of removing them. In my experience, there are usually two reasons for the formation of bubbles after滴ing: one is the滴
When applying the glue, if it is too thick, it may absorb air. Secondly, if the attachment between the picture and the base is not tight, there may be issues.
If there are gaps, glue will seep in and easily create bubbles.If the preparatory work is done well, it can be reduced.
Bubble formation.
7. Methods to remove bubbles: the bubbles inside can be picked out with a toothpick or needle, while the surface bubbles can be blown away using a lighter
Surfaces with bubbles in the glue. If dust gets stuck on them by accident, it can also
Pick it out with the tip of a needle. It is recommended to prepare it in the morning so you can observe it throughout the day for easy correction. As long as the glue has not set.
It’s not too late to fix it once the needle can’t get in!












Ningbo Haishu Xiguan Plastics Products Co., Ltd. is a manufacturer of various thin sheet blister packaging (PVC, PET, PS, PP).(PE) Vacuum forming boxes, flocked vacuum forming, vacuum forming trays, thick sheet vacuum forming, vacuum forming shells, vacuum formed products, edge-capped cylinders, heat shrink filmsFactories specializing in the production, processing, and wholesale of products, with a complete quality management system. Ningbo City Haishu Xiguan PlasticsThe integrity, strength, and product quality of the adhesive products company are recognized in the industry. Friends from all sectors are welcome to visit., guidance and business negotiations.